PAINT TREATMENT Paint treatment ΞΦ95 series 0 1.6 RESPRAYING GLASS-FIBRE REINFORCED POLYESTER PARTS These parts can be recognised by the visible fibre-glass structure on the rear of the part, and the gel coating on the front of the part. 1. Remove any preserving agents, if applicable; see "General operations". 2. Clean the area to be resprayed with a solvent. 3 3. Sand the area to be resprayed first with P80 sand paper and then with P180 sand paper. 4. Remove any dust from the sanded section with a Tack-rag cloth. 5. Fill the area to be resprayed. 6. Leave the filler to dry. 7. Apply spray filler to the part to be resprayed. 8. Leave the spray filler to dry. 9.
Sand the filled area first with P80 sand paper and then with P180 sand paper. 10. Remove any dust from the area to be resprayed with a Tack-rag cloth. 11. Clean the area to be resprayed with a solvent. 12. Again remove any dust from the area to be resprayed with a Tack-rag cloth. 13. Blow ionised air over the area to be resprayed, or clean the area with an anti- static liquid. 14. Apply filler to the area to be resprayed. 15. Leave the filler to evaporate/dry. 16. If necessary, fine-sand with 3M Scotch Brite ultra fine or an equivalent product. 17. Remove any dust from the area to be resprayed with a Tack-rag cloth. 18.
Blow ionised air over the area to be resprayed, or clean the area with an anti- static liquid. 19. Apply the top coat according to the manufacturer's instructions. 20. Leave the top coat to evaporate/dry. Drying temperatures must not exceed 60 % C. Comply with the drying times listed in the manufacturer's instructions. 1-8 © 200651