Return to Master Table of Contents Heat Discoloration Heat discoloration can range from faint yellow to dark blue resulting from overload or incorrect lubrication. Excessive heat can cause softening of races or rollers. To check for loss of temper on races or rollers, a simple file test may be made. A file drawn over a tempered part will grab and cut metal, whereas a file drawn over a hard part will glide readily with no metal cutting. Replace bearing if over heating damage is indicated. Check seals and other related parts for damage. Figure 17 Stain Discoloration Discoloration can range from light brown to black caused by incorrect lubrication or moisture.
if the stain can be removed by light polishing or if no evidence of overheating is visible, the bearing can be reused. Check seals and other related parts for damage. Figure 18 S0302000 Page 13 General Maintenance Procedures