Hood 88.00 Hood Repair Also, grind 1/2 inch (13 mm) inward from all edges on the engine side of the section replace- ment. See Fig. 6 , Ref. C. 1 2 3 4 Slightly taper the outside edge of the ground area on the hood and the inside edge of the ground area on the section replacement. See Fig. 7 , Ref. 3. 5 A f880226b 05/04/94 1 A. Grind a shallow recess one-quarter the depth of the FRP and extending 1/2 inch (13 mm) outward in all directions from the damaged area. 2 1. Section Replacement 2. Gap 3. Slight Taper 4. Hood 5. Engine Side of Hood B Fig. 7, Cutout Area (cross-sectional view) A Also, scuff at least 1 inch (25 mm) in from all sides of the section replacement. See Fig. 6 , Ref. D.
Scuff thoroughly, since this will give the section replacement a surface to which it can stick. Be sure to completely sand off any undercoating sprayed on these areas. 3 9. On the outer sides of both the cutout and the section replacement, bevel the edges about 45 degrees. See Fig. 8 . 4 D C A f880224a 02/09/94 A and C: Use a router to grind away a shallow recess one-quarter the depth of the FRP and extending 1/2 inch (13 mm) away from the edge. B and D: Use 80 to 220-grit sandpaper to scuff the area 1 inch (25 mm) around the damage. 1. Cutout Hole 2. Engine Side of Hood 3. Section Replacement 4. Engine Side of Section Replacement B 1 f880200a 04/19/94 A. Insert section replacement. B.
Bevel outer surface edges on all sides. Fig. 6, Preparing the Section Replacement and Hood Cutout on the Unexposed Side 1. Exposed Side of Hood 8. Use 80 to 220-grit sandpaper to scuff an area at least 1 inch (25 mm) out from all sides of the cutout area. See Fig. 6 , Ref. B. Fig. 8, Areas to be Beveled 10. Gently feather the outer painted surfaces back about 1/2 inch (13 mm) beyond the edges of the repair areas (on both the cutout and the section replacement), using 220-grit or finer sandpaper. Business Class M2 Workshop Manual, Supplement 0, September 200 2 140/5