John Deere 700H Crawler Dozer — Welding Repair of Major Structure

Frame Installation Welding Repair of Major Structure 17 1740 Use one of the following weld processes: 4 CAUTION: Avoid potentially toxic fumes and dust. Hazardous fumes can be generated when paint is heated by welding, soldering, or using a torch. AWS-E-7018 covered electrode with shielded metal arc welding (SMAW) process AWS-ER-70S-3 wire electrode with gas metal arc welding (GMAW) process AWS-E70T-1 or E71T-1 wire electrode with flux core arc welding (FCAW) process. Do all work outside or in a well ventilated area. Dispose of paint and solvent properly. Remove paint before welding or heating: If you sand or grind paint, avoid breathing the dust. Wear an approved respirator.

If you use solvent or paint stripper, remove stripper with soap and water before welding. Remove solvent or paint stripper containers and other flammable material from area. Allow fumes to disperse at least 15 minutes before welding or heating. Preheat area to be repaired to allow better weld penetration. To repair weld metal failure, remove failed weld metal using arc or grinding equipment. Welding Repair of Major Structure—Specification Tensile Strength—Pressure 482.6 mPa (70,000 psi) ........................... Yield Strength—Pressure 413.7 mPa (60,000 psi) .............................. Elongation—Percent 22 ........................................................................

IMPORTANT: Disconnect battery ground strap or turn battery disconnect switch to to prevent voltage spikes through alternator or monitor. Thoroughly clean area to be welded. Preheat structural assemblies to a minimum of 38 ° C (100 ° F). Welding Repair of Major Structure—Specification Structural Assemblies— Minimum Temperature 38 ° C (100 ° F) .................................................... Have only a qualified welder do this job. Connect welder ground clamp close to each weld area so electrical current does not pass through any bearings. Preheat ground engaging tools (cutting edges, skid shoes, and teeth shanks) to 177 ° C (350 ° F).

Welding Repair of Major Structure—Specification Ground Engaging Tools— Temperature 177 ° C (350 ° F) ................................................................. Remove or protect all parts that can be damaged by heat or weld splatter. Connect welder ground clamp close to each weld area so electrical current does not arc inside any bearings. To repair base metal failure remove enough material to allow weld to penetrate to the bottom of crack. Preheat structural assemblies to a minimum of 38 ° C (100 ° F). Preheat ground engaging tools (cutting edges, skid shoes, and teeth shanks) to 177 ° C (350 ° F).

CED,OUTX547,160 –19–21OCT98–1/1 TM1859 (14JUL04) 17-1740-4 700H Crawler Dozer 071404 PN=386