NAVFACENGCOM MIL-HDBK-1001/5A — NAVFACENGCOM MIL-HDBK-1001/5A Roofing and Waterproofing Guide PDF

Downloaded from https://www.everyspec.com MIL-HDBK-1001/5A h) Exterior damage is localized by its closed cell structure; i) Recoating will "renew" the system; some coatings are guaranteed for 10 years. 7.2.2 Disadvantages. Compared with conventional built-up roof systems, sprayed polyurethane foam has some offsetting disadvantages:

a) Added cost of recoating the fluid-applied membrane periodically; b) Greater difficulty in obtaining a level surface and uniform insulation thickness; c) Extremely high dependence on applicator's skill; d) High dependence on good substrate preparation; e) Reduced traffic and impact resistance; f) High vulnerability to degradation in hot, humid climates; g) Vulnerability to bird-pecking. Birds will peck through the outer covering, dig out the foam, and sometimes build nests in the cavity. 7.3 Design Recommendations. Consider both design and field-application requirements. First, consider the following design items: a) Slope of substrate.

Do not rely on applicator varying foam thickness to provide slope-to-drain (minimum 1/2 inch per foot (4 percent) for new construction and 1/4 inch per foot (2 percent) for reroofing); b) Wind uplift resistance conforming to FM requirements; c) Substrate requirements. Most systems prohibit foam application directly to a conventional ribbed steel deck. They require a minimum 3/8 inch (10 millimeters) thick exterior-grade plywood (untreated) fastened to the deck. Fastenings should conform with FM requirements for anchoring insulation boards 27