John Deere 400 6076 — John Deere 400 6076 User Manual

Cylinder Block, Liners, Pistons and Rods/Visually Inspect Cylinder Liners VISUALLY INSPECT CYLINDER LINERS IMPORTANT: If pitting has occurred, check condition of coolant. 1. Inspect exterior length of liner for pitting (A). Check packing step for erosion (B). If pitting or erosion is observed, measure the depth of pits and erosion with a fine wire or needle. Replace piston and liner if: —Pitting depth is one-half liner thickness (C) or more. —Erosion depth is one-half packing step (D) or more. CYLINDER LINER SPECIFICATIONS Cylinder Liner Thickness . . . . . . . . . . . . . . . . . . 6.05—6.15 mm (0.238—0.242 in.) RG4643 -UN-13DEC88 Packing Step Dimension . . . . . . . . . . . . . . . . . .

1.45—1.55 mm (0.057—0.061 in.) NOTE: Liners are reusable if the depth of pits or erosion is less than one-half the amount specified. When installing these liners, rotate 90˚ from original position. The liners should be deglazed and ring sets installed on pistons. 10 19 A—Liner Pitting B—Liner Erosion C—Liner Thickness D—Packing Step RG,CTM42,G10,34-19-22JUL94 2. Visually examine liner ID. Replace piston and liner if: — The crosshatch honing pattern is not visible immediately below the top ring turn-around area. — Liners are pitted or contain deep vertical scratches that can be detected by the fingernail. 3.

Carefully examine liner for signs of fatigue, such as fine cracks in the flange area (A) and cracks in the ring travel area (B). NOTE: Inspect block for cracks or erosion in the O-ring packing areas. See INSPECT AND CLEAN CYLINDER BLOCK, later in this group. RG1188 -UN-13DEC88 (Exaggerated defects) CTM42 (24MAR95) 10-19 6076 Diesel Engines—S.N. (500000— ) RG,CTM61,G10,14-19-22JUL94 160101 PN=104