(c) Grinding the crankshaft The crankshaft journals and crankpins must be refinished to a dimension smaller by 0.100 to 0.120 mm (0.00394 to 0.00472 in.) than the undersize of bearings to be used. Example: If 0.50-mm (0.01969-in.) undersize bearings are to be used: The journals must be refinished to 65 - 0.5 - (0.100 - 0.120) [2.55905 - 0.01969 - (0.00394- 0.00472 in.)] The crankpins must be refinished to 58 - 0.5 - (0.100 - 0.120) [2.28346 - 0.01969 - (0.00394- When grinding the crankpins and journals, be sure to produce the same filler radius (shoulder radiUS) as the original one.
Too small a radius of fillet will result in fatigue failure of crankshaft while too large a fillet radius is sure to cause the bearing to ride on the radius and thereby to result in a bearing failure. Be extremely careful not to grind off the radius part beyond the desired dimension. An over-ground radius part can be corrected only by grinding off the shoulder face and this, if effected, will present problems in obtaining a proper end clearance. 0.00472 in.)] Also check the crankpins and journals for hard- ness. They should have a hardness of 620 or more in terms of Vickers Hardness Number.
If necessary, re-harden the crankpins and journals, and check them for cracks by conducting a magnaflux (magnetic particle) test. Specifications Unit: mm (in.) -30- Undersize Journals to be refinished to 0.25 (0.0098) ! 64 75 -0.015 (25 92 -0.00059) . . -0.035 . 4 1-0.00138 0.50 (0.0197) 6450-0.015 (2 5393To.00059) . -0.035' -0.00138 0.75 (0.0295) 6425 -0.015 (2 52952 -0.00059 ) . -0.035' -0.00138