Freightliner — Freightliner Business Class M2 Workshop Manual

Hood 88.00 Hood Repair WARNING the painted surface. Leave a crowned excess of adhesive, slightly higher than the painted sur- face. NOTE: When using Ashland Pliogrip 7775L, dis- pense the required adhesive from the cartridge in a continuous bead of uniform size and a uni- form green color. Discard the initial few inches of discolored bead. Before starting any hood repair procedure, read the safety precautions in Subject 130 . Failure to be aware of the hazards in using raw materials in working with fiberglass could result in serious and long-term health problems. Surface Damage Repair 6. After the adhesive dries (about 50 minutes), sand it with a hand-held disc pad.

Use 320-grit or finer sandpaper. Feather the edges of the fill so there are no visible sharp edges. Surface damage refers to scratches, chips, or nicks on the outer surface of the hood. Use the following instructions to repair surface damage. 1. Examine the damaged area. If there are cracks, see if they go all the way through the hood. If they do, see "Structural Damage Repair" for in- structions. 7. Clean the area with compressed air. Mask the area, then spot prime and paint it. Use Sherwin Williams BB–11 black conductive primer. See Group 98 for spot-painting instructions. 2. Clean the area with xylene, acetone, or an equivalent grease- and wax-removing solvent. Inspect the area closely.

Structural Damage Repair 3. Using 220-grit or finer sandpaper, remove all of the paint around the damaged area to a distance of about 1-1/2 inches (4 cm). See Fig. 1 . The Preform FRP (fiberglass reinforced plastic) hood consists of a one-piece hood assembly. SMC (sheet molded compound) inner reinforcements are bonded to the engine-side of the hood with a structural adhe- sive. If the hood is damaged, determine which parts are affected. 1 2 If there is damage to any of the reinforcements, the damage is not repairable. For example, if the grille area of the hood is damaged so badly that the rein- forcement bonded inside the grille area is also dam- aged, replace the entire hood assembly.

A If a joint between two reinforcements, or between a reinforcement and the hood skin, has separated and there is no damage at the joint area, the parts can be rebonded. Or, if a part of the hood skin is dam- aged and its adjoining reinforcement(s) aren’t dam- aged, the reinforcement can be separated from the damaged part, the damaged part can be patched, and the reinforcement(s) rebonded in place. f880221b 05/04/94 A. Remove paint and primer 1-1/2 inches (4 cm) around the damaged area. Use 220-grit or finer sandpaper. 3 1. Paint 2. Primer 3. Scratch If a has a small crack or hole, it can be repaired; if it has a puncture or large fracture, it must be replaced. Fig.

1, Damaged Area with Paint and In-Mold Coating Removed For rebonding parts, see "Hood Reinforcement Reb- onding." 4. Using an air nozzle, blow off all dust. 5. Apply Ashland Pliogrip 7775L self-leveling ure- thane adhesive over the non-coated area and spread a thin layer using a squeegee applicator. Cover the entire damaged area, overlapping onto For damage in the form of a crack or small hole, see "Crack or Small Hole Repair." For larger damaged areas, see "Puncture or Large Fracture Repair." Business Class M2 Workshop Manual, Supplement 0, September 200 2 140/1