Cummins — 3666003

Piston C Series Page 1-104 Section 1 - Cylinder Block - Group 01 NOTE: Dimensional inspection of the piston is required only when the cause of the lack of sealing is not apparent. Inspect the piston for damage and excessive wear. Check the top ring grooves, skirt, and pin bore. Inspect the piston for rolled edges on the ring lands. If the ring lands are rolled in, this indicates ring beat-in and can cause loss of sealing. Inspect the piston bowl (1), pin bore (2), and skirt (3) for cracks or damage. NOTE: Do not use pistons with cracks. NOTE: If severe piston damage has occurred, check the turbocharger and other exhaust components for damage from debris.

Measure the piston bore when the piston temperature is at 20°C [68°F]. Piston Pin Bore Inside Diameter mm in 45.01 MIN 1.772 45.03 MAX 1.773 NOTE: Add 0.013 mm [0.0005 in] to the piston pin bore inside diameter per 5°C [10°F] temperature rise up to 32°C [90°F]. The piston pin bore must be checked closer to the outside diameter of the piston since the piston pin bore is tapered. Inspect the piston pin for scratches, grooves, or other damage. Measure the piston pin outside diameter. Piston Pin Diameter mm in 44.99 MIN 1.771 45.00 MAX 1.772 NOTE: Discard the piston pin if it is more than 0.03 mm [0.001 in] out of round.