Section 07 BODY AND HULL Subsection 02 (BODY) WARNING Protect skin, wear gloves when in contact with resin, hardeners and gelcoat. A barrier skin cream may also be used. Do not expose area to open flame or lit cigarette. Some of the materials are flammable. Protect eyes, wear safety glasses when grinding, sanding or spraying. Use a dust mask when sanding or grinding. When spraying wear a respirator or paint mask. Always read warning labels on products. Filling the Cavity The prepared surface must be cleaned with ace- tone on a cloth. Use a gelcoat repair kit. Follow the mixing instructions in the kit when preparing the gelcoat putty.
Carefully mix the required amount while making sure there are no air bubbles in the mixture. With a putty knife, fill the repair area and cover with plastic film. Curing time may depend on tempera- ture, amount of putty and percentage of catalyst. After 2 hours, press lightly on the surface with fingers to test the hardness. When the area be- comes hard, remove the plastic film. TOOLS: - Air mask - Power sander - Buffing pad - Putty knife Sanding Begin block sanding the patch with 320-grit sand- paper until you come close to the original surface. Remove dust with a water soaked cloth and con- tinue sanding with a 400-grit wet paper.
Finish wet sanding with a 600-grit to remove deeper scratches. If needed you can wet sand with finer grit paper such as 1000-grit. - Heavy-duty polisher - Sanding block - Cover sheets - Safety glasses - Paint brush - Scissors - Plastic container (mixing) - Spray gun - Plastic film - Stirring stick - Plastic squeegee - White cloths MATERIALS: Buffing and Waxing Buff the surface using a heavy duty polisher with a buffing pad. Make sure the pad is free of dirt or you may damage the gelcoat. Carefully begin buffing with a white medium compound. Finish off using a fine compound. While buffing, pay close attention to avoid overheating the surface.
- Acetone - Epoxy filler - Cabosil - Masking tape - Cardboard - Liquid gelcoat - Fine compound (white) - Medium compound (white) - Fiberglass cloth - Polyester resin - Fiberglass mat - 24-grit sanding disks Blisters Repair Possible causes: Insert catalyst Improper catalyst/gelcoat ratio. A blister is a visible bump on the watercraft sur- face that may not necessarily come right through the gelcoat layer. In the case of only a few blis- ters, follow the same repair procedure as for air bubbles. If they are numerous and in close con- centration, spray liquid gelcoat to achieve proper repair. This procedure is covered in MINOR GEL- COAT FRACTURES.
- Gelcoat putty - Wax - Sandpaper (100-grit, 220-grit, 320-grit, 400-grit, 600-grit, 1000-grit) Air Bubbles Repair Possible cause: Air pocket trapped between layers of laminate and gelcoat. Preparation of Surface Remove all of the damaged gelcoat surrounding the air bubble with a putty knife or preferably a carbide grinding tip. Make sure all loose and weak areas are completely removed. Sand a small area of the gelcoat surface with 220-grit sandpaper. If needed, sand the cavity itself. These areas must have a rough surface to allow the gelcoat putty to bond properly. Minor Gelcoat Fractures Repair Possible causes: Flexing of fiberglass laminate Gelcoat thickness Direct result of impact.
In case of fractures which have not penetrated past the gelcoat layer, the repair concerns the gel- coat only. If flex cracking or impact are evident, 494 smr2009-042