Cylinder Liners - Cleaning and Inspection (01-06) Cylinder Block N14 Page 1-38 Inspection Visually inspect for pitting or erosion in the crevice seal groove. Replace the liner if pitting or erosion is greater than one-half the width of the crevice seal groove. Visually inspect the outside diameter for excessive cor- rosion or pitting. Pits must not be more than 1.60 mm [0.063-inch] deep. Replace the liner if the pits are too deep or if the corrosion can not be removed with a fine emery cloth. Liners which have light pitting or erosion can be used again, but they must be installed with the pitting or ero- sion positioned in line with the crankshaft.
Visually inspect for cracks on the inside and the outside of the liner. Replace the liner if cracks are found.