Department of Defense MIL-STD-1311D — MIL-STD-1311D Test Methods for Electron Tubes — DoD Standard Manual PDF

Downloaded from https://www.everyspec.com MIL-STD-1311D (OBSOLESCENT) METHOD 4102 OPERATION BUMP (Klystron) 1. Purpose. The purpose of this test is to insure that minor transient shocks do not permanently impair tube performance. 2. Procedure. 2.1. Method of mounting. The tubes shall be mounted as shown on the TSS, under specified test conditions. 2.2 Operation bump. This test shall be made with a pendulum consisting of a steel ball .625 inch (15.88 mm) in diameter suspended by a wire .02-inch (0.5 mm) in diameter, with the distance between the point of suspension and the center of the ball 4.250 inch (107.95 mm), or with an equivalent pendulum.

The ball shall be suspended so that when at rest it touches the tube at approximately one-half the distance between the extreme limits of the tube projecting above the socket. In this position, the point of suspension of the ball shall be directly above the center of the ball. The ball shall be permitted to swing freely through an arc of 60 ° in a plane through the axis of the tube and from such an angle that the ball strikes only the tube envelope. 3. Acceptance criteria. After striking the tube with the ball, the power output or the frequency, or both if specified, shall not change by more than the amount indicated.

The tube shall be considered to have met the test satisfactorily if, after testing in this manner three times, the tube does not fail on any test and if, during this test, the quantity measured does not at any time show a nontransient change of more than the specified amount from the original value. METHOD 4102 4102-1 19 April 1968